We recognized a mistake in the input data for creating the datasheet of the material
IDT-Grooved Gasket with graphite layer-WS 1.4571-3803-KD10-20-30-5.0 mm
In the data of the leakage tests at 10 and 40 bar in the unoading curve starting at 60 MPa there was a gasket stress level indicated with 40 MPa instead of 20 MPa. This mistake influences the characteristics QSmin(L) slightly.
In the attached draft of the revised datasheet the characteristics which will change are highlighted yellow.
IDT-Grooved Gasket with graphite layer-WS 1.4571-3803-KD10-20-30-5.0 mm
In the data of the leakage tests at 10 and 40 bar in the unoading curve starting at 60 MPa there was a gasket stress level indicated with 40 MPa instead of 20 MPa. This mistake influences the characteristics QSmin(L) slightly.