SGL SIGRAFLEX HOCHDRUCK PRO V15011Z3IP 1.5mm
#3
(07-22-2020, 07:21 AM)Teadit Wrote: Maybe we should decide to use the average of 3 E-Modul test at such behaviour (results with runaway values)? Some materials seems to have such trend and more tests would give better results to perform calculations. Third test could be performed by inhouse testing.
Agree with proposal of Teadit.

If Pqr test at 300°C was performed later on other test samples, the result can be slightly different from the first tested samples.
Here I would expect the value of 0,92.
Reply


Messages In This Thread
RE: SGL SIGRAFLEX HOCHDRUCK PRO V15011Z3IP 1.5mm - by Donit - 07-22-2020, 11:37 AM