10-07-2020, 11:15 AM
For Frenzelit novaphit SSTC TA-L with XP 2.0 mm I voted for a leakage cross-check at 40 bar. If this cross-check confirms that the data provided by Frenzelit are within the allowable divergence compared to the cross-check, my vote for the 1.6 mm thick material changes to YES. If the cross-check of the 2.0 mm thick material should show that the allowable divergence is not met, I vote for a leakage cross-check at 40 bar for the 1.6 mm thickness as well.